Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -9.44 °C | 15.0 °F | Approx. Cold test |
Lubriplate 1242 Lithium-Polymer Type Multi-Purpose Grease Highly water resistant and tacky, they are designed for applications were the grease is subjected to heavy pressure and shock loads. This series is available in 3 NLGI densities for a wide range of .. |
|||
Minimum Service Temperature, Air | -9.44 °C | 15.0 °F | |
ConocoPhillips 595 NC Open Gear Lube Description: Conoco Open Gear Lube 595 NC is a black, viscous, semi-fluid product that can be applied via central pumping systems that utilize injectors and nozzles for spray or drip application. Op.. |