Material Notes:
Symbol according to ISO 1043-1: (S/B + PE) Special polystyrene alloy with very high tear strength and high stress- cracking resistances. Particularly suitable for extrusion and thermoforming of fatty foods packaging. Applications: lids multi-layers composite thermoformed containers containers for fats Unfilled. Suitable for Film Extrusion, Thermoforming. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 3.8 %
3.8 %
50 mm/min
Tensile Modulus 1.45 GPa
210 ksi
1 mm/min
Thermal Properties Metric English Comments
Vicat Softening Point 70.0 °C
158 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Dielectric Constant 2.4

@Frequency 100 Hz
2.4

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V