Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded , Polyurethane, TP
Manufacturer A. Schulman, Inc.
Trade Name POLYPUR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Linear Mold Shrinkage 0.00050 - 0.0010 cm/cm

@Thickness 3.20 mm,
Time 259000 sec
0.00050 - 0.0010 in/in

@Thickness 0.126 in,
Time 72.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 137 MPa
19900 psi
ASTM D638
Tensile Modulus 8.25 GPa
1200 ksi
ASTM D638
Flexural Strength 180 MPa
26100 psi
ASTM D638
Flexural Modulus 6.89 GPa
999 ksi
tangent; ASTM D790
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648
Users viewing this material also viewed the following: