Processing Properties Metric English Comments
Melt Temperature 288 - 316 °C
550 - 600 °F
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow
Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted..
Melt Temperature 288 - 316 °C
550 - 600 °F
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Melt Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized
Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Melt Temperature 288 - 316 °C
550 - 600 °F
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release
Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Melt Temperature 288 - 316 °C
550 - 600 °F
Polymer Resources PPX-GP1 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
Melt Temperature 288 - 316 °C
550 - 600 °F
Ravago Manufacturing Americas Hylex® P1010LLT Polycarbonate
Information provided by Ravago.
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 300 TFE 5 SI 2 Polycarbonate (PC), PTFE Lubricated - Silicone Lubricated - WearResistant
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 303 TFE 20 SE Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Self Extinguishing - Bromine/Chlorine Free - UL94 V-0
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 382 HEC FR Polycarbonate (PC) Nickel-Coated Carbon Fiber - EMI/RFI/ESD Protection - Flame Retardant
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 383 TFE 15 FR Polycarbonate (PC), Carbon Fiber - PTFE Lubricated - Flame Retardant - UL94 V-0
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 385 Polycarbonate (PC) Carbon Fiber
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 399 X 129972 C Polycarbonate (PC) Flame Retardant - Transparent
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 399 X 95997 B Polycarbonate (PC), Thermally Conductive - Electrically Conductive
Melt Temperature 282 - 316 °C
540 - 600 °F
RTP Company RTP 4000 ET-1001 L Polyphthalamide (PPA), Impact Modified - Lubricated
Melt Temperature 293 - 316 °C
560 - 600 °F
LTL Color Compounds ColorFast® PC100 Polycarbonate
10 melt standard injection molding gradeAll information provided by LTL Color Compounders, Inc.
Melt Temperature 288 - 316 °C
550 - 600 °F
Mitsubishi Iupilon® S2000UR 9.5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company ESD C 380 FR L Polycarbonate (PC), Carbon Fiber - Flame Retardant - ESD Protection - Electrically Conductive - Lubricated
Melt Temperature 260 - 316 °C
500 - 600 °F
RTP Company RTP 2000 A-670 Polysulfone ABS Alloy
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 300 FR A Polycarbonate (PC), Unreinforced - Flame Retardant - Non-PBBO/E - UL94 V-0
The RTP 300 FR A family of materials offer dimensional stability, rigidity, heat resistance, ignition resistance and excellent impact strength.
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 300 HF L UV Polycarbonate (PC), High Flow - Lubricated - UV Stabilized
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 300 AR 10 Polycarbonate (PC), Aramid Fiber
Melt Temperature 302 - 316 °C
575 - 600 °F
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 302 FR Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E - UL94 V-0
The RTP series of flame retardant, glass fiber reinforced polycarbonate materials offer dimensional stability with improved heat distortion and ignition resistance performance over the base resin.
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 305 TFE 15 FR Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Flame Retardant - Non-PBBO/E
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 387 Polycarbonate (PC), Carbon Fiber
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 399 X 115084 B Polycarbonate (PC), Carbon Nanotube - Static Dissipative - ESD Protection
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 399 X 86846 H Polycarbonate (PC) Flame Retardant - Halogen Free - Transparent
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 399 X 88744 Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Perfluoropolyether Oil
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 399 X 91042 Polycarbonate (PC), Thermally Conductive - Electrically Insulative
Melt Temperature 288 - 316 °C
550 - 600 °F
RTP Company RTP 302 TFE 15 Polycarbonate (PC), Glass Fiber - PTFE Lubricated