Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories SFC-90S High-Alumina Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SFC-90S High-Alumina Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.014715 GPa

@Temperature 110 °C,
Time 86400 sec
2.1343 ksi

@Temperature 230 °F,
Time 24.0 hour
0.021582 GPa

@Temperature 1000 °C,
Time 10800 sec
3.1303 ksi

@Temperature 1830 °F,
Time 3.00 hour
0.022563 GPa

@Temperature 1400 °C,
Time 10800 sec
3.2725 ksi

@Temperature 2550 °F,
Time 3.00 hour
Compressive Strength 78.5 MPa

@Temperature 110 °C,
Time 86400 sec
11400 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
88.3 MPa

@Temperature 1000 °C,
Time 10800 sec
12800 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
98.1 MPa

@Temperature 1400 °C,
Time 10800 sec
14200 psi

@Temperature 2550 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1800 °C
3270 °F
limited
Shrinkage -0.0900 %

@Temperature 1400 °C,
Time 10800 sec
-0.0900 %

@Temperature 2550 °F,
Time 3.00 hour
-0.0600 %

@Temperature 1000 °C,
Time 10800 sec
-0.0600 %

@Temperature 1830 °F,
Time 3.00 hour
-0.0300 %

@Temperature 110 °C,
Time 86400 sec
-0.0300 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 87 %
87 %
SiC 5.0 %
5.0 %
SiO2 5.0 %
5.0 %
Descriptive Properties Value Comments
Installation Method Self Flowing
Material Required for Estimating(kg/?) 3,050
Water Required for Casting(%) 5-5.5