Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Zircar Zirconia Buster M2-35 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast AC 90-5 D Dense Refractory Brick Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast ACZ 85-5 D Dense Refractory Brick Description: Special low porosity quality with excellent resistance against alkali- and metal slags, a good volume stability and a high strength and elasticity at very high temperatures. Application.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast ADHESIET 180 P Dry Air-Setting Refractory Mortar Description: Adhesiet 180 P is a phosphate bonded air setting mortar, supplied as a dry powder. This very pure mortar is for use up to extreme high temperatures.Remarks: Adhesiet mortars can be stor.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast CURON 180 L Dense Refractory Castable Description: Curon 180 L is a castable based on fused alumina for use up to 1800°C and shows a good thermal shock resistance.Remarks: These values apply to cast products. Also available in gunnin.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast CURON 180 TF Dense Refractory Castable Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Momentive Performance Materials HTR1003 PBN/PG Heating Element PBN/PG resistance heating elements combine the unique electrical, chemical, and thermal properties of PBN, a dielectric material, and Pyrolytic Graphite (PG), an electrical conductor, to produce a t.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Momentive Performance Materials HTR1004 PBN/PG Heating Element PBN/PG resistance heating elements combine the unique electrical, chemical, and thermal properties of PBN, a dielectric material, and Pyrolytic Graphite (PG), an electrical conductor, to produce a t.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast AK 99 Dense Refractory Brick Description: This high purity alumina based brick finds wide application in chemical reactors. The low percentages of SiO2 and Fe2O3 makes this brick very resistant in reducing conditions.Remarks: T.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Sharadaa Ceramics REFCAST HA High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Sinotek Materials HFB Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and .. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Sapco 99.9% Aluminum Oxide Information provided by Sapco. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Sharadaa Ceramics REFCAST LC95 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | Continuous |
Unifrax Fibermax® Duraboard® 18H Board Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. .. |
|||
Maximum Service Temperature, Air | 1800 - 1950 °C | 3270 - 3540 °F | Continuous |
Goodfellow Ruby, Al2O3 Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Zircar Ceramics Alumina Furnaceware ZIRCAR Ceramics Alumina Furnaceware are high purity fully dense, fine grain aluminum oxide products suitable for use in applications with temperatures as high as 1800°C. Such uses include crucibles.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories HACT-180 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories HACT-180G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories HSC-18SC Dense and High-Strength Castable, Superdense Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories LPCT-18PI Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories MMCT-95 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories PTF-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories SCX-90IP Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories SFC-90S High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories SFC-90SC High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories SFC-UL90S High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast LP 100 Dense Refractory Brick Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qual.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast FLUCON 180 Dense Self Flowing Refractory Castable Description: Flucon 180 is a self flowing castable based on white fused Alumina. This castable is applied at severe thermal conditions and or severe slag attack.Remarks: These values apply to cast p.. |