Mechanical Properties Metric English Comments
Compressive Strength 78.5 MPa

@Temperature 110 °C
11400 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFCAST LC60 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength 78.5 MPa

@Temperature 110 °C
11400 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFCAST LC70 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength >= 78.5 MPa

@Temperature 110 °C
>= 11400 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics VELCRETE G403 Gunning Castables
Description: Available from us a range of Gunning Castables that are made in compliance with the set industrial standards. These castables are widely used in refineries, foundries, boilers, rolling ..
Compressive Strength 78.5 MPa

@Temperature 1100 °C
11400 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics ZAP 002 Smart Cast Application
Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle working LayerInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 78.5 MPa

@Temperature 110 °C
11400 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics ZAP 003 Smart Cast Application
Special Properties: Anti-repellent PropertiesIndustry: CementApplication: Cement Plant Smoke ChamberInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 78.5 MPa

@Temperature 1500 °C
11400 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics ZAP 005 Smart Cast Application
Special Properties: Non-wetting, Slag and Hot Abrasion ResistanceIndustry: SteelApplication: Trough LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 78.5 MPa

@Temperature 1100 °C
11400 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics ZAP 008 Smart Cast Application
Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle Safety Layer, Sponge Iron Rotary Kiln BackupInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 78.5 MPa

@Temperature 1400 °C
11400 psi

@Temperature 2550 °F
Cold Crushing
Sharadaa Ceramics Sharada RFC-90 Gel Bonded Castables
Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E..
Compressive Strength 78.5 MPa

@Temperature 1500 °C,
Time 10800 sec
11400 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories CTC-65SH Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 78.5 MPa

@Temperature 110 °C,
Time 86400 sec
11400 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 78.5 MPa

@Temperature 110 °C,
Time 86400 sec
11400 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 78.5 MPa

@Temperature 1350 °C,
Time 10800 sec
11400 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories LPCT-17PI Lance Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 78.5 MPa

@Temperature 1500 °C,
Time 10800 sec
11400 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories MMCT-85 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 78.5 MPa

@Temperature 1500 °C,
Time 10800 sec
11400 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories MMCT-95 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 78.5 MPa

@Temperature 110 °C,
Time 86400 sec
11400 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories SCX-60KL Special SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 78.5 MPa

@Temperature 1000 °C,
Time 10800 sec
11400 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SFC-165 High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 78.5 MPa

@Temperature 110 °C,
Time 86400 sec
11400 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories SFC-90S High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved