Polymer Property : Compressive Strength = 88.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 88.3 MPa

@Temperature 150 °C
12800 psi

@Temperature 302 °F
JIS K7208
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Compressive Strength 88.3 MPa

@Temperature 110 °C
12800 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFCAST A SUPER High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Compressive Strength 88.3 MPa

@Temperature 110 °C
12800 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength 88.3 MPa

@Temperature 1400 °C
12800 psi

@Temperature 2550 °F
Cold Crushing
Sharadaa Ceramics Sharada RFC-95 Gel Bonded Castables
Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E..
Compressive Strength 88.3 MPa

@Temperature 1500 °C
12800 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics ZAP 001 Smart Cast Application
Special Properties: Thermal Shock Slag ResistanceIndustry: FoundryApplication Areas: Foundry LaddleInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 88.3 MPa

@Temperature 1500 °C
12800 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics ZAP 006 Smart Cast Application
Special Properties: Thermal Shock, Flame ErosionIndustry: Multi PurposeApplication: Burner Blocks all types of Thermal Shock ApplicationsInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 88.3 MPa

@Temperature 1500 °C
12800 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics ZAP 008 Smart Cast Application
Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle Safety Layer, Sponge Iron Rotary Kiln BackupInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 88.3 MPa

@Temperature 1500 °C
12800 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics ZAP 009 Smart Cast Application
Special Properties: Thermal Shock, Lesser Dross Formation, Non-wetting To AluminumIndustry: Non-FerrousApplication: Aluminum Melting/Holding Furnace, Launders, Risers, Transfer LaddlesInformation pr..
Compressive Strength 88.3 MPa

@Temperature 1100 °C
12800 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics ZAP 011 Smart Cast Application
Special Properties: Thermal Shock, Accretion, Co, Impact ResistanceIndustry: Sponge IronApplication: Sponge Rotary KilnInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 88.3 MPa

@Temperature 1500 °C
12800 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics ZAP 012 Smart Cast Application
Special Properties: Patching At Hot Conditions, Easy InstallationIndustry: All IndustryApplication: All type of Rotary Kilns, AL/CU Melting Furnaces, Rolling Mills, Forgoing Furnaces, IncineratorsIn..
Compressive Strength 88.3 MPa

@Temperature 110 °C,
Time 86400 sec
12800 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HSC-16H-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa

@Temperature 1000 °C,
Time 10800 sec
12800 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HSC-16SF-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa

@Temperature 1000 °C,
Time 10800 sec
12800 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa

@Temperature 1500 °C,
Time 10800 sec
12800 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories MMCT-75 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa

@Temperature 1400 °C,
Time 10800 sec
12800 psi

@Temperature 2550 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SCX-16KL Special SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa

@Temperature 800 °C,
Time 10800 sec
12800 psi

@Temperature 1470 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SCX-70 I Special SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa

@Temperature 800 °C,
Time 10800 sec
12800 psi

@Temperature 1470 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SCX-85 I Special SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa

@Temperature 1000 °C,
Time 10800 sec
12800 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SFC-70 SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa

@Temperature 1000 °C,
Time 10800 sec
12800 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SFC-90S High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 88.3 MPa

@Temperature 149 °C
12800 psi

@Temperature 300 °F
JIS K7208
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled  (discontinued **)
AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber ..