Polymer Property : Modulus of Rupture = 2.1343 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.014715 GPa

@Temperature 1500 °C,
Time 10800 sec
2.1343 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories A50 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.014715 GPa

@Temperature 1350 °C,
Time 10800 sec
2.1343 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories BLC Lance Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.014715 GPa

@Temperature 110 °C,
Time 86400 sec
2.1343 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories CTC-65SH Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.014715 - 0.016677 GPa

@Temperature 1350 °C,
Time 10800 sec
2.1343 - 2.4188 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories HAPT-80S Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.014715 GPa

@Temperature 110 °C,
Time 86400 sec
2.1343 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HSC-16SF-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.014715 GPa

@Temperature 1500 °C,
Time 10800 sec
2.1343 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories LPCT-17PI Lance Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.014715 GPa

@Temperature 1500 °C,
Time 10800 sec
2.1343 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories MMCT-85 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.014715 GPa

@Temperature 1350 °C,
Time 10800 sec
2.1343 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories MMCT-95 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.014715 GPa

@Temperature 1500 °C,
Time 10800 sec
2.1343 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories MMCT-95 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.014715 GPa

@Temperature 250 °C
2.1343 ksi

@Temperature 482 °F
Chosun Refractories SC40 Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.014715 GPa

@Temperature 1350 °C,
Time 10800 sec
2.1343 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories SFC-70R High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.014715 GPa

@Temperature 110 °C,
Time 86400 sec
2.1343 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories SFC-90S High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).