Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.022563 GPa @Temperature 1350 °C, Time 10800 sec |
3.2725 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories SFC-60 SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.022563 GPa @Temperature 1400 °C, Time 10800 sec |
3.2725 ksi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories SFC-90S High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.022563 GPa @Temperature 1000 °C, Time 10800 sec |
3.2725 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SFC-90SC High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |