Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.021582 GPa @Temperature 1500 °C, Time 10800 sec |
3.1303 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories CTC-85TD Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.021582 GPa @Temperature 110 °C, Time 86400 sec |
3.1303 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HSC-18SC Dense and High-Strength Castable, Superdense Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.021582 GPa @Temperature 1000 °C, Time 10800 sec |
3.1303 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SFC-90S High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |