Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.31 g/cc

@Temperature 1500 °C,
Time 10800 sec
0.0835 lb/in³

@Temperature 2730 °F,
Time 3.00 hour
2.52 g/cc

@Temperature 110 °C,
Time 86400 sec
0.0910 lb/in³

@Temperature 230 °F,
Time 24.0 hour
Mechanical Properties Metric English Comments
Compressive Strength 14.7 MPa

@Temperature 1500 °C,
Time 10800 sec
2130 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
19.6 MPa

@Temperature 110 °C,
Time 86400 sec
2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage -1.50 %

@Temperature 1500 °C,
Time 7200 sec
-1.50 %

@Temperature 2730 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 54 %
54 %
SiO2 16 %
16 %
Descriptive Properties Value Comments
Chemical Analysis(%),SiC+C 23
Installation Method Ramming
Main Applications Min runner
Material Required for Estimating (kg/?) 2,600