Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering Perlast® G80A Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name Perlast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering Perlast® G80A Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Do not use any Perlast ® grade with molten alkali metals.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
°IRHD; ASTM D1415
80
80
°IRHD, 0 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 18.779 MPa
2723.7 psi
-11% change after 72 hours @ 250°C; ASTM D412
21.1 MPa
3060 psi
ASTM D412
Elongation at Break 120 %
120 %
ASTM D412
174 %
174 %
45% change after 72 hours @ 250°C; ASTM D412
100% Modulus 0.00968 GPa
1.40 ksi
-45% change after 72 hours @ 250°C; ASTM D412
0.0176 GPa
2.55 ksi
ASTM D412
Compression Set 15 %
15 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -15.0 °C
5.00 °F
Flash Point >= 400 °C
>= 752 °F