Mechanical Properties Metric English Comments
Compressive Strength 14.7 MPa

@Temperature 200 °C
2130 psi

@Temperature 392 °F
Cold Crushing
Sharadaa Ceramics Sharada LTM 1.4 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 14.7 MPa

@Time 86400 sec
2130 psi

@Time 24.0 hour
Cold Crushing
Sharadaa Ceramics ZAP 001 Smart Cast Application
Special Properties: Thermal Shock Slag ResistanceIndustry: FoundryApplication Areas: Foundry LaddleInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 14.7 MPa

@Time 86400 sec
2130 psi

@Time 24.0 hour
Cold Crushing
Sharadaa Ceramics ZAP 005 Smart Cast Application
Special Properties: Non-wetting, Slag and Hot Abrasion ResistanceIndustry: SteelApplication: Trough LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 14.7 MPa

@Time 86400 sec
2130 psi

@Time 24.0 hour
Cold Crushing
Sharadaa Ceramics ZAP 006 Smart Cast Application
Special Properties: Thermal Shock, Flame ErosionIndustry: Multi PurposeApplication: Burner Blocks all types of Thermal Shock ApplicationsInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 14.7 MPa

@Time 86400 sec
2130 psi

@Time 24.0 hour
Cold Crushing
Sharadaa Ceramics ZAP 008 Smart Cast Application
Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle Safety Layer, Sponge Iron Rotary Kiln BackupInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 14.7 MPa

@Temperature 1500 °C,
Time 10800 sec
2130 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories AN-210 Blast Furnace Runner Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 24.5 MPa

@Temperature 1350 °C,
Time 10800 sec
2130 - 3560 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PT-150 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 24.5 MPa

@Temperature 1350 °C,
Time 10800 sec
2130 - 3560 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PT-170 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
2130 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PTF-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 MPa

@Temperature 1350 °C,
Time 10800 sec
2130 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories CT-130 Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 24.5 MPa

@Temperature 1350 °C,
Time 10800 sec
2130 - 3560 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PT-140 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 24.5 MPa

@Temperature 110 °C,
Time 86400 sec
2130 - 3560 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HACT-150 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 24.5 MPa

@Temperature 1000 °C,
Time 10800 sec
2130 - 3560 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-150 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 24.5 MPa

@Temperature 1000 °C,
Time 10800 sec
2130 - 3560 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-155 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 24.5 MPa

@Temperature 1350 °C,
Time 10800 sec
2130 - 3560 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-160 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 24.5 MPa

@Temperature 110 °C,
Time 86400 sec
2130 - 3560 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HACT-160 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 19.6 MPa

@Temperature 1000 °C,
Time 10800 sec
2130 - 2840 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-165 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 24.5 MPa

@Temperature 1350 °C,
Time 10800 sec
2130 - 3560 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PT-150 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).