Assab Steels RAMAX 2 Plastic Mold Material

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Assab Steels
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Assab Steels RAMAX 2 Plastic Mold Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stainless steel for holder blocks with excellent machinability and corrosion resistance.Applications: Holders/bolsters for plastic moulds, plastic and rubber moulds with low requirements on polishability, dies for plastic extrusion and constructional parts.
Mechanical Properties Metric English Comments
Hardness, Brinell 300 - 340
300 - 340
hardness supplied.
Component Elements Properties Metric English Comments
Carbon, C 0.28 %
0.28 %
Chromium, Cr 16.7 %
16.7 %
Iron, Fe 81.8 %
81.8 %
Manganese, Mn 1.1 %
1.1 %
Sulfur, S 0.12 %
0.12 %