Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 14.7 MPa @Temperature 200 °C |
2130 psi @Temperature 392 °F |
Cold Crushing |
Sharadaa Ceramics Sharada LTM 1.4 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 14.7 MPa @Time 86400 sec |
2130 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics ZAP 001 Smart Cast Application Special Properties: Thermal Shock Slag ResistanceIndustry: FoundryApplication Areas: Foundry LaddleInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 14.7 MPa @Time 86400 sec |
2130 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics ZAP 005 Smart Cast Application Special Properties: Non-wetting, Slag and Hot Abrasion ResistanceIndustry: SteelApplication: Trough LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 14.7 MPa @Time 86400 sec |
2130 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics ZAP 006 Smart Cast Application Special Properties: Thermal Shock, Flame ErosionIndustry: Multi PurposeApplication: Burner Blocks all types of Thermal Shock ApplicationsInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 14.7 MPa @Time 86400 sec |
2130 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics ZAP 008 Smart Cast Application Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle Safety Layer, Sponge Iron Rotary Kiln BackupInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 14.7 MPa @Temperature 1500 °C, Time 10800 sec |
2130 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories AN-210 Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1350 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-150 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1350 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-170 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 19.6 MPa @Temperature 110 °C, Time 86400 sec |
2130 - 2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PTF-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 MPa @Temperature 1350 °C, Time 10800 sec |
2130 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CT-130 Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1350 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-140 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 110 °C, Time 86400 sec |
2130 - 3560 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-150 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1000 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-150 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1000 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-155 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1350 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-160 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 110 °C, Time 86400 sec |
2130 - 3560 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-160 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 19.6 MPa @Temperature 1000 °C, Time 10800 sec |
2130 - 2840 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 14.7 - 24.5 MPa @Temperature 1350 °C, Time 10800 sec |
2130 - 3560 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-150 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |