Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | >= 19.6 MPa @Temperature 110 °C |
>= 2840 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics PHOSTCAST 60 XL Phosphate Bonded Castables Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and .. |
|||
Compressive Strength | 19.6 MPa @Time 86400 sec |
2840 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST C SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 19.6 MPa @Time 86400 sec |
2840 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST K High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 19.6 MPa @Time 86400 sec |
2840 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST LC45 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 19.6 MPa @Temperature 800 °C |
2840 psi @Temperature 1470 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST LT Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | 19.6 MPa @Time 86400 sec |
2840 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST ULCC90 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 19.6 MPa @Temperature 200 °C |
2840 psi @Temperature 392 °F |
Cold Crushing |
Sharadaa Ceramics Sharada LTM 1.5 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 19.6 MPa @Time 86400 sec |
2840 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST C High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 19.6 MPa @Time 86400 sec |
2840 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST HA PLUS High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 19.6 MPa @Time 86400 sec |
2840 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST LC95 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 19.6 MPa @Temperature 110 °C, Time 86400 sec |
2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories AN-210 Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 MPa @Temperature 500 °C, Time 10800 sec |
2840 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories APC-50 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 MPa @Temperature 500 °C, Time 10800 sec |
2840 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories APC-80G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 MPa @Temperature 110 °C, Time 86400 sec |
2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories CTC-60TD Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 MPa @Temperature 110 °C, Time 86400 sec |
2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories CTC-63TD Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 MPa @Temperature 110 °C, Time 86400 sec |
2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories CTL-Z1 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 110 °C, Time 86400 sec |
2840 - 4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1000 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 110 °C, Time 86400 sec |
2840 - 4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HAPT-80S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1350 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1350 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1500 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-170 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1500 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 350 °C, Time 86400 sec |
2840 - 4270 psi @Temperature 662 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories SCX-90IP Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1000 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-150S High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 MPa @Temperature 110 °C, Time 86400 sec |
2840 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories TCH-175SV Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1350 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-155 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 110 °C, Time 86400 sec |
2840 - 4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-155 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1350 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 110 °C, Time 86400 sec |
2840 - 4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |