Material Notes:
Finished product available in rods.Chicago Extruded Metal temper code: M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 7.20 g/cc
0.260 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 29
29
Tensile Strength 689 MPa
100000 psi
Tensile Strength, Yield 379 MPa
55000 psi
Elongation at Break 1.0 %
1.0 %
Thermal Properties Metric English Comments
Thermal Conductivity 34.6 W/m-K
240 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Aluminum, Al 12.5 - 13.5 %
12.5 - 13.5 %
Copper, Cu >= 78.5 %
>= 78.5 %
as balance
Iron, Fe 3.5 - 5.5 %
3.5 - 5.5 %
Manganese, Mn <= 2.0 %
<= 2.0 %
Other, total 0.50 %
0.50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000172 ohm-cm
0.0000172 ohm-cm