China Tungsten YG9X Tungsten Carbide Powder

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YG9X Tungsten Carbide Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by China Tungsten
Physical Properties Metric English Comments
Bulk Density 3.20 g/cc
0.116 lb/in³
Scott
Density 14.6 g/cc
0.527 lb/in³
Binder 2.0
2.0
wax
Particle Size 0.80 µm
0.80 µm
Mechanical Properties Metric English Comments
Hardness, Rockwell A 92
92
Tensile Strength, Ultimate 2000 MPa
290000 psi
Component Elements Properties Metric English Comments
Cobalt, Co 9.0 %
9.0 %
Other 0.20 %
0.20 %
WC 90.8 %
90.8 %
Descriptive Properties Value Comments
Flow Rate; sec/50g 30