Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | pressed |
PPT LSF120 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | pressed |
PPT LSF16 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | pressed |
PPT LSF180 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | pressed |
PPT LSF220 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | pressed |
PPT LSF25 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | pressed |
PPT LSF400 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | pressed |
PPT LSF50 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | |
MarkeTech Repton 115 Aluminum Oxide Brand 115 features: High Density and Purity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even whe.. |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | |
Zircar Ceramics DAHP Dense Alumina Hearth Plate ZIRCAR Dense Alumina Hearth Plates are used for supporting loads in high temperature furnaces and other thermal process systems. These dense plates are made of fully sintered fine grain high purity .. |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | |
China Tungsten YG15C Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | |
China Tungsten YG6X Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | Scott |
China Tungsten YG9 Tungsten Carbide Powder Information provided by China Tungsten |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | Scott |
China Tungsten YG9X Tungsten Carbide Powder Information provided by China Tungsten |
|||
Bulk Density | 3.21 g/cc | 0.116 lb/in³ | |
Chosun Refractories AB10H Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | |
Chosun Refractories AB10S Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | |
Chosun Refractories BTB-18S Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | |
Chosun Refractories CRZG-L30 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | |
Chosun Refractories SAL95 Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | |
Chosun Refractories SAL99C Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 3.20 g/cc | 0.116 lb/in³ | Scott |
China Tungsten YG9C Tungsten Carbide Powder Information provided by China Tungsten |