Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Greene Tweed Avalon® 16 PTFE, Glass, Molybdenum Filled

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer Greene Tweed
Trade Name Avalon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Avalon® 16 PTFE, Glass, Molybdenum Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin to reinforced, exhibit low friction while being chemically inert. Avalon thermoplastics can be custom designed to for each unique application.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.27 g/cc
2.27 g/cc
ASTM D792
Deformation 20 %
20 %
2000 psi 78°F; ASTM D621
30 %
30 %
1000 psi 300°F; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Yield 19.48 MPa
2825 psi
ASTM D1457
Elongation at Break 247 %
247 %
ASTM D1457
Compressive Strength 26.2 MPa
3800 psi
ASTM D695
Shear Strength 14.5 MPa

@Temperature 149 °C
2100 psi

@Temperature 300 °F
ASTM D732
15.9 MPa

@Temperature 93.3 °C
2300 psi

@Temperature 200 °F
ASTM D732
17.6 MPa

@Temperature 65.6 °C
2550 psi

@Temperature 150 °F
ASTM D732
19.3 MPa

@Temperature 37.8 °C
2800 psi

@Temperature 100 °F
ASTM D732
20.0 MPa

@Temperature 26.7 °C
2900 psi

@Temperature 80.0 °F
ASTM D732
Coefficient of Friction, Static 0.10
0.10
33.3 psi
K (wear) Factor 18.1 x 10-8 mm³/N-M
9.00 x 10-10 in³-min/ft-lb-hr
Descriptive Properties Value Comments
Color Dark Gray to Black
Copyright © lookpolymers.com All Rights Reserved