Physical Properties Metric English Comments
Density 14.6 g/cc
0.527 lb/in³
PSM Industries PolyAlloys MIM-WC-9Co Tungsten Carbide
Information Provided by PolyAlloys, a division of PSM Industries
Density 14.6 g/cc
0.527 lb/in³
Wieland 1907 Wilaform Gold
Palladium white gold alloy with beautiful grey-white color.Applications: casting, chains, laminar decoration, pipes, tubingDental
Density 14.6 g/cc
0.527 lb/in³
China Tungsten YG546 Tungsten Carbide
Good toughness, high strength, capable of resisting high impact load, Roughing of stainless steel and cast irons.Information provided by China Tungsten
Density 14.6 - 15.0 g/cc
0.527 - 0.542 lb/in³
China Tungsten YG6 Cemented Tungsten Carbide for Mining Purposes
For coring crowns, electric coal drill bits, coal cutting picks. oil cone bits and scraping knife bits used in geological prospecting, coal mining and oil well boringInformation provided by China Tu..
Density 14.6 - 15.0 g/cc
0.527 - 0.542 lb/in³
China Tungsten YG6 Tungsten Carbide for Dies and Wear Part Making
For drawing of steels, non-ferrous metal and alloy bars of
Density 14.6 g/cc
0.527 lb/in³
China Tungsten YG9X Tungsten Carbide Powder
Information provided by China Tungsten
Density 14.6 - 14.9 g/cc
0.527 - 0.538 lb/in³
China Tungsten YGR8 Tungsten Carbide with Rare Earth Additive
Higher wear resistance, service strength and impact toughness than YG6 and YG8. For drawing of steel
Density 14.6 g/cc
0.527 lb/in³
China Tungsten ZK40 Tungsten Carbide
High in strength and impact resistance, Roughing and strength cutting of cast iron.Information provided by China Tungsten
Density 14.6 g/cc
0.527 lb/in³
China Tungsten YG524 Tungsten Carbide
High strength alloy with high toughness and impact resistance ,for milling and planning of large bamboo and wood surfaces.Information provided by China Tungsten
Density 14.6 g/cc
0.527 lb/in³
China Tungsten YG610 Tungsten Carbide
Good thermal strength and high wear resistance .Continuous or intermittent  cutting of cast irons, refractory alloys and quenched steelInformation provided by China Tungsten
Density 14.6 - 15.0 g/cc
0.527 - 0.542 lb/in³
China Tungsten YG6X Tungsten Carbide for Dies and Wear Part Making
For drawing of steel wires and non-ferrous metal wires or bars of