Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Particle Size = 0.80 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.80 µm
0.80 µm
Median Diameter
Omya OMYAPAQUE® Calcium Carbonate
An ultrafine ground calcium carbonate for paper and board filling. An opacifying product that is designed to reduce costs through the replacement of more expensive pigments.Information supplied by O..
Particle Size 0.80 - 1.5 µm
0.80 - 1.5 µm
d50
Magyar Aluminum ALOLT 120F Aluminum Hydroxide
Fine Precipitated Type
Particle Size 0.80 µm
0.80 µm
Average Particle Size/Laser Diffraction D50
H.C. Starck Grade HD 15 Boron Carbide, B4C
Powder for sintering.Abrasive grit or powder (grinding, lapping, polishing)Wear resistant engineering components (e.g. sand-blasting and water jet nozzlesLight weight ceramic armorMetal infiltration..
Particle Size 0.80 µm
0.80 µm
Average Particle Size/Laser Diffraction D50
H.C. Starck Grade HS Boron Carbide, B4C
Powder for sintering.Abrasive grit or powder (grinding, lapping, polishing)Wear resistant engineering components (e.g. sand-blasting and water jet nozzlesLight weight ceramic armorMetal infiltration..
Particle Size 0.80 - 1.1 µm
0.80 - 1.1 µm
d10
Indium Corp. In(OH)3 Fine Indium Hydroxide
Indium Acetate is a white powder. Fine Powder Form: Primary particles range from 0.1 to 1.0 microns in size. they range in shape from spherical to elliptical to cylindrical. Agglomerates can be ..
Particle Size 0.80 - 1.8 µm
0.80 - 1.8 µm
Average Particle Size/Laser Diffraction D50
H.C. Starck Grade C Aluminum Nitride AIN
High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon..
Particle Size 0.80 - 1.2 µm
0.80 - 1.2 µm
Average
H.C. Starck Grade C Titanium Nitride
Additive for ceramic parts to increase electrical conductivityConstituent for cermets and black ceramicsRaw material for TiN sputter targets
Particle Size 0.80 µm
0.80 µm
Solvay Chemicals Blanc fixe brilliant
Blanc Fixe Brilliant is the optimal extender for almost all applications in the production of paints and coatings and plastic.Information provided by Solvay
Particle Size 0.80 µm
0.80 µm
Shin-Etsu Silicones X-52-854 Fluid
Information Provided by Shin-Etsu Silicones of America, Inc.
Particle Size 0.80 µm
0.80 µm
Rubber Particle Size
UBE B (Low-Cis) HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %)
Description: UBE high impact polystyrene (HIPS).Information provided by UBE.
Particle Size 0.80 µm
0.80 µm
d10
TIMCAL TIMREX® HSAG400 Primary Synthetic High Surface Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 0.80 µm
0.80 µm
d10
TIMCAL TIMREX® HSAG500 Primary Synthetic High Surface Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 0.80 µm
0.80 µm
Rubber Particle Size
UBE UBEPOL BR13HB HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %)
Description: UBEPOL-BR13HB is characterized by its low solution viscosity compared with conventional grades and short dissolution time in styrene monomer. Its main merits are as follows:Short dissol..
Particle Size 0.80 µm
0.80 µm
China Tungsten YG11X Tungsten Carbide Powder
Information provided by China Tungsten
Particle Size 0.80 µm
0.80 µm
China Tungsten YG13X Tungsten Carbide Powder
Information provided by China Tungsten
Particle Size 0.80 µm
0.80 µm
China Tungsten YG9X Tungsten Carbide Powder
Information provided by China Tungsten
Particle Size 0.80 µm
0.80 µm
China Tungsten YG15X Tungsten Carbide Powder
Information provided by China Tungsten
Particle Size 0.80 µm
0.80 µm
China Tungsten YG6X Tungsten Carbide Powder
Information provided by China Tungsten
Copyright © lookpolymers.com All Rights Reserved