Material Notes:
D870 = Transparent Amorphous Nylon for Injection Molding, Unlubricated. D870L = Transparent Amorphous Nylon for Injection Molding, Lubricated.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 97.0 MPa
14100 psi
ASTM D638
Elongation at Break 150 %
150 %
Flexural Modulus 3.20 GPa
464 ksi
ASTM D790
Izod Impact, Notched 0.720 J/cm
1.35 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 119 °C
246 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 109 °C
228 °F
ASTM D648
Optical Properties Metric English Comments
Refractive Index 1.58
1.58
ASTM D542
Transmission, Visible 85 %
85 %
ASTM D1003
Processing Properties Metric English Comments
Processing Temperature 275 - 315 °C
527 - 599 °F