ChevronTexaco Starplex® Moly NLGI Grade 2

Category Fluid , Lubricant , Lithium Gellant
Manufacturer ChevronTexaco Corp
Trade Name Starplex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Starplex® Moly NLGI Grade 2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending vehicle life.Heat resistance with excellent high temperature properties.Good low temperature pumpability — Better low temperature performance means better handling in the container and grease-dispensing equipment.Molybdenum disulfide for additional boundary lubrication protection.Texaco Starplex Moly greases are multipurpose, water resistant, extreme pressure greases intended primarily for use in construction, mining and agricultural applications.They are manufactured using selected highly refined high viscosity index base oils, a lithium complex soap, a 1.5% molybdenum disulfide ("moly") antiwear agent, plus oxidation and rust inhibitors. They are dark gray in color and tacky in texture.Texaco Starplex Moly greases are available in two grades:NLGI 1 for better pumpability at low ambient temperaturesNLGI 2 for normal ambient temperatures.Texaco Starplex Moly greases are designed especially for use in construction, mining and agricultural applications. They can also provide longer mileage life in king pins, spring shackles, and steering system bearings on over-the-road trucks and other offhighway equipment. Texaco Starplex Moly greases strongly resist being washed out of bearings. They are stable and retain their consistency under adverse service conditions, and protect parts over long service intervals. Texaco Starplex Moly greases have outstanding film strength and adhesive properties which result in particularly effective protection in shock loadand extreme pressure service. The antiwear properties provided by the lithium complex thickener are enhanced by the molybdenum disulfide. They may also be used in automotive wheel bearing and chassis lubrication.Texaco Starplex Moly greases are recommended as multipurpose products for the lubrication of both over-the-road and off-highway trucks, tractors, and heavy duty equipment. They give excellent performance in all automotive equipment in severe service. They provide top protection to fifth wheels, king pins, wheel bearings, steering system bearings, and all chassis points including ball joints and universal joints. They also perform well in most heavy-duty industrial applications for general lubrication and for the lubrication of journal bearings, and low and moderate speed antifriction bearings. They are particularly effective in applications where a high dropping point and high EP are desirable.They perform well under high temperature, wet, and dusty operating conditions.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication. Determined on mineral oil extracted by vacuum filtration.CPS Number: 221944; MSDS Number: 8804
Physical Properties Metric English Comments
Viscosity Measurement 117
117
Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 1681 SUS
1681 SUS
See Note 3.
Saybolt Viscosity at 210°F 144 SUS
144 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 32 cSt
32 cSt
See Note 3.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
Four Ball Wear 0.500 mm
0.0197 in
Scar Diameter
Penetration P(0), 1/10 mm 264
264
Unworked, 25°C (77°F)
Penetration P(60), 1/10 mm 274
274
Unknown Amount of Work, 25°C (77°F)
Timken Test 18100 g
40.0 lb
OK Load
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
See Note 2.
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
See Note 1.
Dropping Point 270 °C
518 °F
Descriptive Properties Value Comments
Thickener, % 12
Lithium Complex