Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Recommended |
Nye Lubricants 797 (NC346) (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | See Note 1. |
ChevronTexaco Coupling Grease NLGI Grade 0/1 Texaco Coupling Grease delivers value through:Superior film strength — Formulated with a high viscosity base oil and polymer for superior film strengthLittle to no oil separation in high-speed coup.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Application; ASTM C1299 |
3M 3000WT Fire Barrier Water Tight Sealant 3M Fire Barrier Water Tight Sealant 3000 WT is a high-performance, ready-to-use, single component, neutral cure, non-slumping intumescent silicone sealant. Product cures upon exposure to atmospheric.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M 7052 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7045 and 7052 are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FA032 Matte Clear Acetate Label Products 3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM012R Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM065 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM118K Indoor UL Recognized MC Polyester Label Products 3M™ Indoor UL Recognized MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These po.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM152 Indoor UL Recognized Computer Imprintable Silver Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM157P Indoor UL Recognized Computer Imprintable Silver Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM1732R White Polyester Label Products 3M™ White Polyester Label Products FM1732 and FM1732R are durable, high performance materials that offer excellent thermal stability. These polyester label products utilize 3M™ Adhesive R3500, whi.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM28J Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FV291 White Vinyl Label Products 3M™ White Vinyl Label Products FV291 and FV292 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl label products utilize 3M™ Adhesive P14.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FV292 White Vinyl Label Products 3M™ White Vinyl Label Products FV291 and FV292 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl label products utilize 3M™ Adhesive P14.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FV365 Soft Yellow Vinyl Label Products 3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FV512 Semi-Rigid Vinyl Label Product 3M™ Semi-Rigid Vinyl Label Products are semi-rigid white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1410, which is a general purpose.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FVT30E Tire Label Product 3M™ Tire Label Products utilize a flexible and conformable white vinyl labelstock that offers durability, moisture resistance, and dimensional stability. 3M™ Adhesive G1120, a rubber-based aggress.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Application |
3M OFM0101 Outdoor UL Recognized Polyester Overlaminate Label Products 3M™ Outdoor UL Recognized Polyester Overlaminate Label Products are durable high performance clear materials that offer excellent thermal stability, abrasion and moisture resistance. These polyeste.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Application |
3M OFM0109 Outdoor UL Recognized Polyester Overlaminate Label Products 3M™ Outdoor UL Recognized Polyester Overlaminate Label Products are durable high performance clear materials that offer excellent thermal stability, abrasion and moisture resistance. These polyeste.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M 7911FL Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM022R Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM055 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM12E Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FM155 Indoor UL Recognized Computer Imprintable Silver Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M FP029202 White Polypropylene Label Product 3M™ White Polypropylene Label Products FP02750N and FP029202 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480 which is a high performance tackifi.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Application |
3M OFM010N Outdoor UL Recognized Polyester Overlaminate Label Products 3M™ Outdoor UL Recognized Polyester Overlaminate Label Products are durable high performance clear materials that offer excellent thermal stability, abrasion and moisture resistance. These polyeste.. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M OFM1502 Outdoor UL Recognized Clear Polyester Label Product 3M™ Outdoor UL Recognized Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M P1510 Medical Permanent Acrylic Adhesives 3M™ Medical Permanent Acrylic Adhesives P1510 demonstrates excellent peel and tack performance and are designed for use in the medical attachment market.Information provided by 3M |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | |
3M 3635-20b Diffuser Film Control light transmission or achieve special effects for backlit signs; 2 and 4-mil vinyl film; Pressure-sensitive adhesive and Adheres to rigid or flexible substratesInformation provided by 3M |
|||
Minimum Service Temperature, Air | -29.0 °C | -20.2 °F | Service |
3M OFL0109 Outdoor UL Recognized Lexan Label Products 3M™ Outdoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P.. |