Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 222 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips SUPER-STA NLGI No. 2 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2783 |
ConocoPhillips Syncon® 220 Synthetic EP Gear Oil, AGMA No. 5EP Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2783 |
ConocoPhillips Syncon® 320 Synthetic EP Gear Oil, AGMA No. 6EP Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips Syncon® Extra Long Life Grease NLGI No. 00 Description: Conoco Syncon Extra Long Life Grease is an ultra high performance lithium-complex grease with heavy synthetic base oil specifically designed for long service life under heavily loaded c.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ConocoPhillips Tacna® HD Grease NLGI Grade 1 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D-2596 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 0 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D-2596 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 1 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco 100 NC Open Gear Lubricant FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco FM Grease EP Aerosol FeaturesChevron FM Grease EP Aerosol is a high performance multipurpose food machinery grease. It is off white in color, tasteless, water-resistant, smooth and buttery in texture, and slightly tacky.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco NLGI 0 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco NLGI 1 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco NLGI 2 Moly Grease EP FeaturesChevron Moly Greases EP are general purpose, extreme pressure (EP) greases. They are manufactured using highly refined selected base oils, a lithium-12-hydroxystearate thickener, 3% molybden.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco RPM® NLGI 1 Automotive LC Grease EP FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco RPM® NLGI 2 Automotive LC Grease EP FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco RPM® NLGI 2 Heavy Duty LC Grease EP FeaturesChevron RPM Heavy Duty LC Greases EP are multipurpose, water resistant, extreme pressure, heavy duty chassis, wheel bearing, and general purpose lubricating greases.They are manufactured usi.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Starplex® Moly NLGI Grade 1 Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending veh.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Starplex® NLGI Grade 2 Texaco Starplex greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protectio.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 111 Mobilux EP Mobilux EP 111 is an extra high performance grease primarily designed for lubrication of all designs of couplings. It is specifically formulated to resist centrifugal separation of the oil from the .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 221 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 222 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 222 Special Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 223 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil Mobilgrease XTC Mobilgrease XTC is an extra high performance product designed for use in high speed coupling applications. It is manufactured with a selected high viscosity mineral base oil and an extremely effecti.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Load |
ConocoPhillips EP Conolith® HT Grease NLGI NO. 1 Description: Conoco EP Conolith HT Grease is a premium-quality, lithium-complex, multipurpose, extreme-pressure, high-temperature grease developed to satisfy the severe requirements of high-speed wh.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 1000, AGMA Number 8A EP Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 680, AGMA Number 8EP Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips SUPER-STA M NLGI No.0 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco Ulti-Plex® NLGI 0 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Aerosol Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |