Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 102 Mobilgrease EAL Mobilgrease EAL 101 and 102 are supreme performance greases designed specifically for applications which are environmentally sensitive. These products are biodegradable and virtually non-toxic greas.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 222 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 222 Special Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2783 |
ConocoPhillips Syncon® 460 Synthetic EP Gear Oil, AGMA No. 7EP Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D974 |
ConocoPhillips Syncon® 680 Synthetic EP Gear Oil, AGMA No. 8EP Description: Conoco Syncon Synthetic EP Gear Oil is a synthetic polyalphaolefin (PAO) lubricant for enclosed gear sets requiring extreme-pressure gear oils and operating at high temperatures. It is .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D-2596 |
ConocoPhillips Syncon® EP Heavy Duty Grease NLGI 2 Description: Conoco Syncon EP Heavy Duty Grease is an ultra high-performance synthetic base oil, lithium-complex grease specifically designed for extreme loading conditions. The combination of high-.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips Syncon® Extra Long Life Grease NLGI No. 00 Description: Conoco Syncon Extra Long Life Grease is an ultra high performance lithium-complex grease with heavy synthetic base oil specifically designed for long service life under heavily loaded c.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ConocoPhillips Tacna® HD Grease NLGI Grade 2 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco FM NLGI 1 Grease EP FeaturesChevron FM Greases EP are high performance, multipurpose food machinery greases that are white in color, odorless, tasteless, and water-resistant. Available in three grades, Chevron FM Greas.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D 2783 |
ChevronTexaco Havoline® SAE 80W-90 Gear Oil Havoline Gear Oils are multipurpose lubricants. They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protection and long lubricant life.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D 2783 |
ChevronTexaco Havoline® SAE 85W-140 Gear Oil Havoline Gear Oils are multipurpose lubricants. They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protection and long lubricant life.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Multifak® EP NLGI Grade 1 Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Multifak® EP NLGI Grade 2 Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco NC Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco NLGI 0 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco NLGI 1 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Starplex® NLGI Grade 2 Texaco Starplex greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protectio.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 103 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil Mobilgrease XTC Mobilgrease XTC is an extra high performance product designed for use in high speed coupling applications. It is manufactured with a selected high viscosity mineral base oil and an extremely effecti.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Load |
ConocoPhillips EP Conolith® HT Grease NLGI NO.2 Description: Conoco EP Conolith HT Grease is a premium-quality, lithium-complex, multipurpose, extreme-pressure, high-temperature grease developed to satisfy the severe requirements of high-speed wh.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 1000, AGMA Number 8A EP Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 460, AGMA Number 7EP Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips SUPER-STA M NLGI No.2 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips Tacna® 2000 NLGI No. 1 Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D-2596 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 2 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 461 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco Ulti-Plex® NLGI 0 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil Mobilgrease XTC Mobilgrease XTC is an extra high performance product designed for use in high speed coupling applications. It is manufactured with a selected high viscosity mineral base oil and an extremely effecti.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Aerosol Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |