Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 270 °C
518 °F
ASTM D2265
ExxonMobil Mobil Polyrex EM 103
Super-premium Mobil Polyrex EM Series grease is specially formulated for electric-motor bearings. The advanced thickener formulation and proprietary manufacturing techniques provide improved bearing..
Dropping Point 270 °C
518 °F
ConocoPhillips Tacna® EP Polyurea Grease NLGI Grade 1
Description: Conoco Tacna EP Polyurea Grease is a shear-stable product with exceptional extreme-pressure characteristics and excellent water resistance. It is recommended for use in steel mills, off..
Dropping Point 270 °C
518 °F
ChevronTexaco Molytex® EP NLGI Grade 2
Texaco Molytex EP grease delivers value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading, extending vehicle ..
Dropping Point 270 °C
518 °F
ChevronTexaco RPM® NLGI 1 Automotive LC Grease EP
FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,..
Dropping Point 270 °C
518 °F
ChevronTexaco RPM® NLGI 2 Automotive LC Grease EP
FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,..
Dropping Point 270 °C
518 °F
ChevronTexaco RPM® NLGI 2 Heavy Duty LC Grease EP
FeaturesChevron RPM Heavy Duty LC Greases EP are multipurpose, water resistant, extreme pressure, heavy duty chassis, wheel bearing, and general purpose lubricating greases.They are manufactured usi..
Dropping Point 270 °C
518 °F
ChevronTexaco Starplex® Moly MPGM 2
Texaco Starplex Moly MPGM grease delivers value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading, extending ..
Dropping Point 270 °C
518 °F
ChevronTexaco Starplex® NLGI Grade 2
Texaco Starplex greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protectio..
Dropping Point 270 °C
518 °F
ASTM D2265
ExxonMobil Mobil Polyrex EM 103
Super-premium Mobil Polyrex EM Series grease is specially formulated for electric-motor bearings. The advanced thickener formulation and proprietary manufacturing techniques provide improved bearing..
Dropping Point 270 °C
518 °F
ChevronTexaco Starplex® Moly NLGI Grade 2
Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending veh..
Dropping Point 270 °C
518 °F
ChevronTexaco Starplex® NLGI Grade 1
Texaco Starplex greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protectio..