Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication. Determined on mineral oil extracted by vacuum filtration.Unknown amount of work.CPS Number: 222336; MSDS Number: 10957
Physical Properties Metric English Comments
Viscosity Measurement 10
10
Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 131 SUS
131 SUS
See Note 3.
Saybolt Viscosity at 210°F 40 SUS
40 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 25 cSt
25 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
See Note 3.
Mechanical Properties Metric English Comments
Penetration 5.0
5.0
% Change, (10000X), 25°C, See Note 4.
Penetration P(0), 1/10 mm 415
415
Unworked, 25°C (77°F)
Penetration P(60), 1/10 mm 415
415
25°C (77°F)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
See Note 2.
Minimum Service Temperature, Air -35.0 °C
-31.0 °F
See Note 1.
Pour Point -40.0 °C
-40.0 °F
See Note 3.
Flash Point 168 °C
334 °F
See Note 3.
Dropping Point 162 °C
324 °F
Descriptive Properties Value Comments
Color Light Green
Texture Smooth
Thickener, % 3.5
Lithium