Material Notes:
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce HDPE, IPQ employs Hoechst/Hostalen technology through the following steps: the ethene supplied by COPESUL is processed by Ipiranga Petroquímica in reactors to produce powdered polyethylene. The polyethylene then receives additives and is homogenized with stabilizers and taken to extruding presses where it is granulated and is ready for marketing.An integrated and computerized system controls the production, from the initial processing stages to end-product testing for later commercialization.Applications:geomembranesjacketing of optics and metallic cables (telecommunicationpipes for irrigation and miningsheets for thermoforming
Physical Properties Metric English Comments
Density 0.944 - 0.948 g/cc
0.0341 - 0.0342 lb/in³
ASTM D792-98
Melt Flow 0.34 - 0.56 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.34 - 0.56 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238-00
High Load Melt Index 8.0 - 14 g/10 min

@Load 21.6 kg,
Temperature 190 °C
8.0 - 14 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238-00
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638-02
Elongation at Yield 9.8 %
9.8 %
ASTM D638-02
Flexural Modulus 0.810 GPa
117 ksi
2% secant; ASTM D790-02
Izod Impact, Notched 2.70 J/cm
5.06 ft-lb/in
ASTM D256-03
Users viewing this material also viewed the following: