Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pacific Sintered Materials BZN-131-U Nickel Silver Powdered Metal

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Pacific Sintered Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pacific Sintered Materials BZN-131-U Nickel Silver Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Higher strength than brass. Good corrosion resistance.Equivalent MPIF Specification: CZN-1818-17All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.60 - 7.80 g/cc
0.275 - 0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell H 80
80
Tensile Strength, Ultimate 234 MPa
34000 psi
Tensile Strength, Yield 138 MPa
20000 psi
Elongation at Break 11 %
11 %
Flexural Strength 503 MPa
73000 psi
Transverse Rupture
Charpy Impact, Unnotched 32.5 J
24.0 ft-lb
Electrical Properties Metric English Comments
Electrical Resistivity 0.000034 ohm-cm
0.000034 ohm-cm
Descriptive Properties Value Comments
Electrical Conductivity (% IACS) 5
Users viewing this material also viewed the following: