Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 40 SUS | 40 SUS | |
ChevronTexaco CP Grease FeaturesChevron CP Grease is a corrosion preventive grease.It is manufactured with a special low viscosity, low pour point base oil, a lithium thickener, and rust and oxidation inhibitors. It is lig.. |
|||
Saybolt Viscosity at 210°F | 40 SUS | 40 SUS | See Note 3. |
ChevronTexaco MCP Grease L NLGI Grade 00 Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe.. |
|||
Saybolt Viscosity at 210°F | 40 SUS | 40 SUS | |
ChevronTexaco ParaLux® 1001 Paraffinic Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |
|||
Saybolt Viscosity at 210°F | 40 SUS | 40 SUS | |
ChevronTexaco ParaLux® 1001R Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |
|||
Saybolt Viscosity at 210°F | 40 SUS | 40 SUS | |
ChevronTexaco ParaMount™ 1001 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
Saybolt Viscosity at 210°F | 40 SUS | 40 SUS | |
ChevronTexaco ParaMount™ 1005 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
Saybolt Viscosity at 210°F | 40 SUS | 40 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® FGC 5 Fluid, Synthetic Mechanical Seal Fluid ISO 22 Description: ANDEROL FGC 5 Mechanical Seal Fluid is a synthetic hydrocarbon (PAO) based lubricant. FGC 5 Fluid meets the former H-1 approval requirements of the USDA where incidental food contact ca.. |
|||
Saybolt Viscosity at 210°F | 40 SUS | 40 SUS | |
ConocoPhillips Sulnap® 22 Cutting Oil Description: Conoco Sulnap Cutting Oil is suited for general-purpose machining operations, such as turning, boring, planing, shaping, light- to medium-duty threading, sawing, hobbing and gear cuttin.. |