Material Notes:
The VH-08 dust filter assemblies are constructed from three layers of corrugated aluminum mesh held in a ‘C’ section aluminum extruded frame. Please see standard profiles available in our catalogue. For protection of the mesh an expanded aluminum kick plate is fitted within the frame. It is recommended that these units are used in conjunction with fan assisted forced air ventilation.Information provided by P & P Technology
Electrical Properties Metric English Comments
Shielding Effectiveness 42 dB

@Frequency 10000 Hz
42 dB

@Frequency 10000 Hz
H-Field
43 dB

@Frequency 1.00e+10 Hz
43 dB

@Frequency 1.00e+10 Hz
E-Field
52 dB

@Frequency 1.00e+9 Hz
52 dB

@Frequency 1.00e+9 Hz
E-Field
53 dB

@Frequency 100000 Hz
53 dB

@Frequency 100000 Hz
H-Field
60 dB

@Frequency 1.00e+8 Hz
60 dB

@Frequency 1.00e+8 Hz
E-Field
61 dB

@Frequency 1.00e+6 Hz
61 dB

@Frequency 1.00e+6 Hz
H-Field
81 dB

@Frequency 1.00e+7 Hz
81 dB

@Frequency 1.00e+7 Hz
E-Field
92 dB

@Frequency 1.00e+6 Hz
92 dB

@Frequency 1.00e+6 Hz
E-Field