Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Chemlon 256 Nylon 6, Wire Jacketing Grade

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced, Flame Retardant
Manufacturer Chem Polymer
Trade Name Chemlon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 256 Nylon 6, Wire Jacketing Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A non-halogenated, Allwires rated wire coating grade used primarily on cables for power and control circuits in commercial and industrial applications. The cables are oil, gasoline, and abrasion resistant, and exceed the requirements of UL Standard 83.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.0 MPa
2470 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 27.6 MPa
4000 psi
ASTM D790
Flexural Modulus 0.600 GPa
87.0 ksi
ASTM D790
Izod Impact, Notched 1.06 J/cm
1.99 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Processing Properties Metric English Comments
Melt Temperature 240 °C
464 °F