Material Notes:
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as cost-effective extruded and dry-pressed forms. 701 offers very good thermal shock resistance, good flexural strength, and 0–1% porosity due to its vitrified properties. This cordierite can self-glaze. It is suitable for applications such as commercial heater supports.
Physical Properties Metric English Comments
Density 2.50 g/cc
0.0903 lb/in³
DIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 0.00 - 1.0 %
0.00 - 1.0 %
DIN EN 623-2 / ASTM-C373
Mechanical Properties Metric English Comments
Vickers Microhardness 670
670
HV 0.5; DINV ENV 843-4
Tensile Strength at Break 27.5 MPa
3990 psi
ACMA Test #4 / DIN EN 843-1
Tensile Modulus 130 GPa
18900 ksi
Young's; DINV ENV 843-2 / ASTM-F417
Flexural Strength 103 MPa
14900 psi
20 x 40 mm
Compressive Strength 344 MPa
49900 psi
ASTM C-773-88 / DIN 51067T1
Poissons Ratio 0.30
0.30
DINV ENV 843-2
Shear Modulus 53.0 GPa
7690 ksi
Thermal Properties Metric English Comments
CTE, linear 2.40 µm/m-°C

@Temperature 20.0 - 200 °C
1.33 µin/in-°F

@Temperature 68.0 - 392 °F
3.30 µm/m-°C

@Temperature 20.0 - 600 °C
1.83 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C373
3.90 µm/m-°C

@Temperature 20.0 - 1000 °C
2.17 µin/in-°F

@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.700 J/g-°C

@Temperature 100 - 200 °C
0.167 BTU/lb-°F

@Temperature 212 - 392 °F
DINV ENV 821-3
Thermal Conductivity 3.20 W/m-K
22.2 BTU-in/hr-ft²-°F
DIN EN 821-2 / ASTM-C408
Maximum Service Temperature, Air 1100 °C
2010 °F
Electrical Properties Metric English Comments
Volume Resistivity 19000 ohm-cm

@Temperature 900 °C
19000 ohm-cm

@Temperature 1650 °F
770000 ohm-cm

@Temperature 500 °C
770000 ohm-cm

@Temperature 932 °F
2.50e+11 ohm-cm

@Temperature 100 °C
2.50e+11 ohm-cm

@Temperature 212 °F
IEC 672-1
1.00e+14 ohm-cm

@Temperature 25.0 °C
1.00e+14 ohm-cm

@Temperature 77.0 °F
ASTM-D257
Dielectric Constant 5.3

@Frequency 1.00e+6 Hz
5.3

@Frequency 1.00e+6 Hz
IEC 672-1 / ASTM-C150
Dielectric Strength 7.874 kV/mm
200.0 kV/in
6.35 mm (1/4") IEC 672-1
Dielectric Loss Index 0.025

@Frequency 1.00e+6 Hz
0.025

@Frequency 1.00e+6 Hz
IEC 672-1 / ASTM-D149,150
Descriptive Properties Value Comments
Color Light Gray
Te Value (°C) 485
Thermal Shock Resistance R1 (K) 600
Hasselman (Experimental)