Electrical Properties Metric English Comments
Dielectric Strength 7.874 kV/mm
200.0 kV/in
6.35 mm (1/4") IEC 672-1
CeramTec 701 Cordierite
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c..
Dielectric Strength 7.874 kV/mm
200.0 kV/in
6.35 mm (1/4") IEC 672-1
CeramTec 975 Alumina, 99.5%
975 (99.5%) offers unique technology by virtue of its optimal dispersion of the MgO phase with the alumina grains. With virtually no transgranular porosity in its microstructure, 975 exhibits high d..