Thermal Properties Metric English Comments
CTE, linear 3.30 µm/m-°C

@Temperature 20.0 - 600 °C
1.83 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C373
CeramTec 701 Cordierite
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c..
CTE, linear 3.30 µm/m-°C

@Temperature 20.0 - 200 °C
1.83 µin/in-°F

@Temperature 68.0 - 392 °F
CeramTec GRADE A LAVA Machinable Ceramic
GRADE A LAVA is a machineable ceramic that exhibits good electrical and heat resistance. It is excellent in applications where close tolerances must be held. This material is available in a variety ..