Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 2.40 µm/m-°C @Temperature 20.0 - 200 °C |
1.33 µin/in-°F @Temperature 68.0 - 392 °F |
|
CeramTec 701 Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |