Material Notes:
CAPILENE® T 77 A is a high melt flow rate polypropylene homopolymer for injection molding with nucleation and antistatic additivation. It exhibits good stiffness, combined with good thermal stability and short molding cycles. APPLICATIONS CAPILENE ® T 77 A is designed for household articles, closures, crates, containers and garden furniture. It is frequently used in blends with a heterophasic copolymer.
Physical Properties Metric English Comments
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.80 GPa
261 ksi
ASTM D790
Izod Impact, Notched 0.250 J/cm

@Temperature >=23.0 °C
0.468 ft-lb/in

@Temperature >=73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ASTM D1525