Material Notes:
This material has good machinability and can be bonded or welded. Its applications include sliding bearings, hammerheads, and toothed gears.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 2.3 %
2.3 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 6.5 %
6.5 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 88

@Thickness 10.0 mm
88

@Thickness 0.394 in
ISO 2039-2
Ball Indentation Hardness 165 MPa
23900 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 85.0 MPa
12300 psi
v = 50 mm/min; ISO 527-2
Elongation at Break 25 %
25 %
ISO 527-2
Tensile Modulus 3.50 GPa
508 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
Melting Point 220 °C
428 °F
10K/min; ISO 3146
Maximum Service Temperature, Air 105 °C
221 °F
Long Term
170 °C
338 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75-2
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
HB

@Thickness 6.00 mm
HB

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
IEC 60250
3.6

@Frequency 100 Hz
3.6

@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm
635 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.012

@Frequency 100 Hz
0.012

@Frequency 100 Hz
IEC 60250
0.016

@Frequency 1e+6 Hz
0.016

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112