Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 101R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 201R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. Internal mold release. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 203R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Europe-Africa-Middle East) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E1530 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-12 SI® High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | DOM 52612 |
Manifattura Cattaneo PA 6 G Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV8111 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV8112 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Haysite H258 Polyester Laminate Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C-177 |
Glastic SG-200 Corner Angles Corner angles used for coil winding.Information provided by Glastic Corporation |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon PUR Polyurethane Very high wear resistanceHighly resilientInformation provided by Isoflon. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV567 Translucent Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 2410F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). UL94 V0 and 5VA listing. US FDA and European Food contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA (Asia Pacific) LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM PW2300 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Shin-Etsu Silicones KE-1204 BL Silicone, Potting/Encapsulation RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Trelleborg Emerson & Cuming Stycast® XT-1122 Two-Component Epoxy Flexible Encapsulant Emerson & Cuming XT-1122 Stycast® Two-Component Epoxy Flexible EncapsulantHeat, thermal shock and impact resistance. Good chemical resistance, Low Viscosity, Unfilled. Mix Ratio (by weight) = 100:6.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Dow CYCLOTENE™ 3022-35 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Staramide B28N PA6, Nucleated, Injection Molded Staramide B28N is a Nucleated and Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Elisto THERMOSTAR® HD 800 Frame Press Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Starflam B28UL PA6, Flame Retardant, Injection Molded Starflam B28UL is Unfilled Halogen Free and Red Phosphorous Free, Flame Retardant, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E 1530 |
Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E 1530 |
Arlon 51228R015 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E1530 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | Result based on 450G; ISO/CD 22007-4 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | Estimated from similar grades. |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | Average; ISO 22007-4 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |