Budd Hi-Flex® SMC  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Polyester, TS
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Budd Hi-Flex® SMC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Parts requiring high strength and dimensional stability, excellent surface smoothness without sink marks; parts to be painted requiring an automotive-type finish.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
Water Absorption <= 0.45 %
<= 0.45 %
ASTM D570-63
Linear Mold Shrinkage 0.00060 cm/cm
0.00060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 73.0 MPa
10600 psi
ASTM D638-68
Flexural Yield Strength 126 MPa
18300 psi
ASTM D790-70
Flexural Modulus 6.25 GPa
906 ksi
Izod Impact, Notched 11.0 J/cm
20.6 ft-lb/in
ASTM D256-70
Thermal Properties Metric English Comments
CTE, linear 10.1 µm/m-°C

@Temperature 23.0 - 150 °C
5.61 µin/in-°F

@Temperature 73.4 - 302 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 235 °C
>= 455 °F
ASTM D648-61