Polymer Property : Tensile Strength, Ultimate = 73.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 73.0 MPa
10600 psi
ISO 527
LATI LATILUB 88/50-30GRT PEEK Based, 30% Graphite and PTFE Self Lubricating Plastic  (Unverified Data**)&l
Latilub self-lubricating plastic materials are designed to replace metals in applications such as gears, bushings, cams, slides, etc., for which, besides their intrinsic properties (moldability, low..
Tensile Strength, Ultimate 73.0 - 130 MPa
10600 - 18900 psi
Average value: 106 MPa Grade Count:4
Overview of materials for PCT, 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr..
Tensile Strength, Ultimate 73.0 MPa
10600 psi
ISO 527
LATI LATAN 13 G/15 15% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)  (discontinued **)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Tensile Strength, Ultimate 73.0 MPa
10600 psi
Lucite International Lucite® 47G Acrylic Bead Resin
Lucite® 47G is usually processed as a glass separation resin and has major particle size distribution between 80-100 mesh. It is a methyl methacrylate copolymer.General Lucite® Acrylic Bead R..
Tensile Strength, Ultimate 73.0 MPa
10600 psi
ASTM D638
Lucky CF-920 Acrylic
May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.
Tensile Strength, Ultimate 73.0 MPa
10600 psi
ASTM D638
Lucky EG-920 Acrylic, Extrusion Grade
Special extrusion grade with excellent stress cracking resistance, intended mainly for exterior applications. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, hi..
Tensile Strength, Ultimate 73.0 MPa
10600 psi
ASTM D638
Plenco 6015 Phenolic, Briquette, Injection Molded
PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf..
Tensile Strength, Ultimate 73.0 MPa

@Temperature 704 °C
10600 psi

@Temperature 1300 °F
AK Steel 409 ULTRA FORM® Stainless Steel
AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and ..
Tensile Strength, Ultimate 73.0 MPa
10600 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 123 Polypropylene, Glass Reinforced, Chemically Coupled, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 73.0 MPa
10600 psi
ASTM D638
Asahi Kasei Delpet® 80N Acrylic Molding Compound, High Heat Grade
80N has high heat resistance and strength. Recommended for taillight lenses, reflectors, and other auto parts, and general lighting fixtures. General Delpet® qualities include attractive transpar..
Tensile Strength, Ultimate 73.0 MPa
10600 psi
ASTM D638-68
Budd Hi-Flex® SMC  (discontinued **)
Parts requiring high strength and dimensional stability, excellent surface smoothness without sink marks; parts to be painted requiring an automotive-type finish.Data provided by the manufacturer.