Polymer Property : Linear Mold Shrinkage = 0.00060 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00060 cm/cm
0.00060 in/in
ATM D955
Plenco 51240 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..
Linear Mold Shrinkage 0.00060 cm/cm
0.00060 in/in
Momentive Performance Materials RTV8262 Silicone Rubber Compounds for Potting, Encapsulating and Sealing
RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr..
Linear Mold Shrinkage 0.00060 - 0.0030 cm/cm
0.00060 - 0.0030 in/in
Lehmann & Voss LUVOCOM® 1105/XCF/20 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Linear Mold Shrinkage 0.00060 - 0.0030 cm/cm
0.00060 - 0.0030 in/in
Lehmann & Voss LUVOCOM® 1105/XCF/25 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Linear Mold Shrinkage 0.00060 - 0.0030 cm/cm
0.00060 - 0.0030 in/in
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Linear Mold Shrinkage 0.00060 - 0.0030 cm/cm
0.00060 - 0.0030 in/in
Lehmann & Voss LUVOCOM® 1105-7536 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Linear Mold Shrinkage 0.00060 cm/cm
0.00060 in/in
average process; in flow; 150x80x2mm
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced
Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre..
Linear Mold Shrinkage 0.00060 cm/cm
0.00060 in/in
flex bar; ASTM D955
Lubrizol ESTALOC® 60204 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
Linear Mold Shrinkage 0.00060 cm/cm
0.00060 in/in
Compression Molding; ISO 2577
Sumitomo Bakelite North America RX® 655 Novolac Phenolic
Fiberglass and mineral reinforced phenolic molding compound with very high fill level (75%). Excellent dimensional stability and good strength at elevated temperatures. Very low thermal expansion ..
Linear Mold Shrinkage 0.00060 cm/cm
0.00060 in/in
Budd Hi-Flex® SMC  (discontinued **)
Parts requiring high strength and dimensional stability, excellent surface smoothness without sink marks; parts to be painted requiring an automotive-type finish.Data provided by the manufacturer.
Linear Mold Shrinkage 0.00060 cm/cm
0.00060 in/in
ATM D955
Plenco 51015 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by..