Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem H 501 HC Bioriented Film Polypropylene

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem H 501 HC Bioriented Film Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: High stiffness; barrier films for conversionInformation provided by Braskem
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792A
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 2.04 GPa
296 ksi
ASTM D790
Izod Impact, Notched 0.310 J/cm

@Temperature 23.0 °C
0.581 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ASTM D648
Vicat Softening Point 158 °C
316 °F
-1kg; ASTM D1525