Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, at 50% RH
(d AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature 23.0 °C |
0.581 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LATAMID 12 H FE85 Nylon 12 Base Magnetizable Compound
(discontinued **) Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 A |
Metabolix Mirel™ F1006 Injection Molding Grade PHA Bioplastic Mirel F1006 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 A |
Metabolix Mirelâ„¢ P1004 Injection Molding Grade PHA Bioplastic Mirel P1004 is a general purpose injection molding grade with high toughness.About Mirel BioplasticsMirel is a family of bioplastic materials that have physical properties comparable to petroleum-ba.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature -30.0 °C |
0.581 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature 23.0 °C |
0.581 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature 23.0 °C |
0.581 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66 LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 9405H-1 Glass Filled Electrical Encapsulation Grade Epoxy E-9504H-1 is glass fiber filled epoxy molding compound designed for encapsulation of delicate electrical components as well as large coils. Excellent thermal shock, moldability, and retention of ele.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature -30.0 °C |
0.581 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UX08325 PPA (Asia Pacific) LNP* Thermocomp* UX08325 is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring)application. Additional feature is high heat. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL EFN4230 PPE+PS (Asia Pacific) PPE+PS high heat transparent grade |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature -30.0 °C |
0.581 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature -30.0 °C |
0.581 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
Plenco 7591 Phenolic, Pellet, Transfer Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | |
Abatron AboCast 50-3/AboCure 50-17 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Dark Amber color. Shelf life is 12+ months. |
|||
Izod Impact, Notched | 0.310 - 5.30 J/cm | 0.581 - 9.93 ft-lb/in | Average value: 0.762 J/cm Grade Count:14 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature 23.0 °C |
0.581 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 501 HC Bioriented Film Polypropylene Applications: High stiffness; barrier films for conversionInformation provided by Braskem |