Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem BI 818 LDPE Injection Molding Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem BI 818 LDPE Injection Molding Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Injection molding; masterbatches. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
ESCR 100% Igepal® 1.0 hour

@Thickness 3.00 mm,
Temperature 23.0 °C
1.0 hour

@Thickness 0.118 in,
Temperature 73.4 °F
compression molded plaques; ASTM D1693
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 45
45
ASTM D2240
Tensile Strength at Break 10.0 MPa
1450 psi
ASTM D638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 615 %
615 %
ASTM D638
Secant Modulus 0.149 GPa
21.6 ksi
0.01; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 8.5 %
8.5 %
60° angle; ASTM D2457