Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | <= 1.0 hour | <= 1.0 hour | F50; ASTM D1693B |
SABIC M300054 High Density Polyethylene for Injection Molding Product Description: M300054 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow.. |
|||
ESCR 100% Igepal® | 1.0 hour @Thickness 3.00 mm, Temperature 23.0 °C |
1.0 hour @Thickness 0.118 in, Temperature 73.4 °F |
compression molded plaques; ASTM D1693 |
Braskem BI 818 LDPE Injection Molding Polyethylene
(discontinued **) Applications: Injection molding; masterbatches. Information provided by Braskem |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
ESCR 100% Igepal® | <= 1.0 hour @Temperature 50.0 °C |
<= 1.0 hour @Temperature 122 °F |
F<sub>50</sub>; Compression molded; ASTM D1693 |
Dow 620I Linear Low Density Polyethylene (LDPE) For extruded foam applications Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
ESCR 100% Igepal® | <= 1.0 hour @Temperature 50.0 °C |
<= 1.0 hour @Temperature 122 °F |
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693 |
Dow 722 Linear Low Density Polyethylene (LDPE) DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c.. |
|||
ESCR 100% Igepal® | <= 1.0 hour @Temperature 50.0 °C |
<= 1.0 hour @Temperature 122 °F |
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693 |
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-9810 NT 7 is produced using UNIPOL™ PE process technology and is supplied in pellet form. This resin is specifically designed as a carrier resin for color concentrates and other masterbat.. |
|||
ESCR 100% Igepal® | <= 1.0 hour @Temperature 50.0 °C |
<= 1.0 hour @Temperature 122 °F |
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693 |
Dow 959S Linear Low Density Polyethylene (LDPE) DOW Polyethylene 959S is a medium molecular weight distribution homopolymer. This resin has good process-ability over a wide range of molding conditions. Typical applications include lids. It com.. |
|||
ESCR 100% Igepal® | <= 1.0 hour @Temperature 50.0 °C |
<= 1.0 hour @Temperature 122 °F |
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693 |
Dow DNDB-1077 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-1077 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
ESCR 100% Igepal® | 1.0 hour | 1.0 hour | Condition B; ASTM D1693 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |