Isoflon Tisoflon® 10K Polytetrafluoroethylene Coated Kevlar Fabric

Category Polymer , Thermoset , Aramid
Manufacturer Isoflon
Trade Name Tisoflon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon Tisoflon® 10K Polytetrafluoroethylene Coated Kevlar Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PTFE coated Kevlar fabric TISOFLON®Information provided by Isoflon.
Physical Properties Metric English Comments
Thickness 285 microns
11.2 mil
Coating Weight 490 g/m²
306 lb/ream
entire thickness; NF EN ISO 2286.2
Mechanical Properties Metric English Comments
Tear Strength 73.0 - 88.0 kN/m
417 - 502 pli
NF EN ISO 1421
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Descriptive Properties Value Comments
PTFE Content (%) 55